← Back to search

Reducing Toxic Thallium in Tl-2223 Cuprate

R. Shipra, Athena S. Sefat

arXiv:1506.02995 · DOI 10.1016/j.physc.2015.09.006 · 2015-06-09

T1theoretical

Active bibliographic source — not scientific approval

Bibliographic access preserves source history; it does not approve extracted materials or validate reported claims. Review warnings on each occurrence separately.

Abstract

The present study gives an account of the effect of Li2O on the ease of phase formation and superconducting properties of Tl2Ba2Ca2Cu3O10+x (Tl-2223) material. Li substitution only slightly decreases the superconducting transition temperature, while the optimal concentration of 20% doping improves the critical current density (Jc) by ~ two fold. We found substantial effects on the synthesis temperature, microstructure and normal state transport properties of Tl-2223 with Li2O addition. Short-time thermal annealing under flowing Ar+4%H2 (1 hr.) further improves the superconducting volume fractions, as well as Jc.

Source-reported materials — not catalogue approval

FormulaReported Tc (K)Pressure (GPa)Type
Tl2Ba2Ca2Cu3O10+x

Archive — visibility unverified

Source-occurrence policy only; no material identity or catalogue acceptance is inferred from the formula.

—Pressure not reportedunknown

Similar papers