Abstract

The complex dielectric constant $\hatε = ε_1 + i ε_2$ of SrTiO$_3$ reaches high values $ε_1 \approx 2*10^{4}$ at cryogenic temperatures, while the dielectric losses ($ε_2$) are much stronger than for other crystalline dielectrics. SrTiO$_3$ is a common substrate for oxide thin films, like the superconducting LaAlO$_3$/SrTiO$_3$ system, but the large $ε_1$ and $ε_2$ restrict high-frequency quantum devices on SrTiO$_3$. Here we present superconducting coplanar Nb resonators on SrTiO$_3$, which we successfully operate in a distant-flip-chip geometry at frequencies that exceed 1 GHz. We find a pronounced and unexpected increase in resonator quality factor $Q$ at temperatures below 1 K, reaching up to $Q \approx 800$. We attribute this to substantial changes of the dielectric losses in SrTiO$_3$ at mK temperatures, and we also detect non-monotonous changes in the temperature-dependent $ε_1$. These findings challenge our present understanding of the dielectric properties of SrTiO$_3$ and at the same time demonstrate that cryogenic high-frequency devices on SrTiO$_3$ are more feasible than previously assumed.

Source-reported materials — not catalogue approval

FormulaReported Tc (K)Pressure (GPa)Type
Nb

Archive — visibility unverified

Source-occurrence policy only; no material identity or catalogue acceptance is inferred from the formula.

7.5Pressure not reportedunknown

Similar papers