Tc max
10.4 K
Tc ambient
10.4 K
Discovery
1998
Papers
15
Tc max measured at ambient, single_crystal, resistivity, arXiv:cond-mat/0105335, confirmed by 3 papers
Evidence (18 records from 15 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Paper |
|---|---|---|---|---|---|---|
| 10.4 | ambient | — | — | — | 2002 | cond-mat/0202442 |
| 10.4 | ambient | single_crystal | resistivity | — | 2001 | cond-mat/0105335 |
| 10.4 | ambient | single_crystal | thermal_conductivity, resistivity | d-wave | 2001 | cond-mat/0107537 |
| 10.0 | ambient | single_crystal | resistivity | — | 2002 | cond-mat/0201567 |
| 10.0 | ambient | single_crystal | susceptibility | — | 2000 | cond-mat/0001149 |
| 9.6 | ambient | single_crystal | resistivity | — | 2001 | cond-mat/0105335 |
| 9.5 | ambient | single_crystal | — | — | 2003 | cond-mat/0302244 |
| 9.2 | ambient | single_crystal | susceptibility | — | 2003 | cond-mat/0311300 |
| 9.0 | ambient | single_crystal | susceptibility | d-wave | 2001 | cond-mat/0108376 |
| 8.9 | ambient | single_crystal | susceptibility | — | 2003 | cond-mat/0311300 |
| — | ambient | — | STM | d-wave | 2003 | cond-mat/0306551 |
| — | — | single_crystal | resistivity | — | 2002 | cond-mat/0203392 |
| — | ambient | — | susceptibility | — | 2002 | cond-mat/0208012 |
| — | ambient | single_crystal | resistivity | — | 2001 | cond-mat/0104570 |
| — | ambient | single_crystal | susceptibility | — | 2001 | cond-mat/0105335 |
| — | ambient | — | — | d-wave | 2000 | cond-mat/0006327 |
| — | ambient | — | — | d-wave | 1999 | cond-mat/9912254 |
| — | ambient | single_crystal | resistivity | d-wave | 1998 | cond-mat/9805354 |
Structure
- Crystal structure
- κ
- Lattice c (Å)
- 16.200
Superconducting parameters
- Pairing symmetry
- d-wave
- Gap structure
- nodal
- Hc2
- 35.0 T (at 2 K)
- λ_eph (e–ph coupling)
- —
Competing orders
- Competing order
- AFM
Samples & pressure
- Sample form
- single_crystal
- Pressure type
- none