Tc max
4.7 K
Tc ambient
4.7 K
arXiv year
2014
Papers
1
Tc exp.
4.7 K
Tc theo.
—
Evidence
experimental
Tc max measured at single_crystal, susceptibility, DOI: 10.1103/PhysRevB.90.020505
Evidence (4 records from 1 paper)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 4.7 | — | single_crystal | susceptibility, resistivity | — | 2014 | T1 | DOI: 10.1103/PhysRevB.90.020505 |
| 4.0 | — | single_crystal | resistivity | — | 2014 | T1 | DOI: 10.1103/PhysRevB.90.020505 |
| 3.4 | — | single_crystal | resistivity | — | 2014 | T1 | DOI: 10.1103/PhysRevB.90.020505 |
| 3.2 | — | single_crystal | resistivity | — | 2014 | T1 | DOI: 10.1103/PhysRevB.90.020505 |
Structure
- Crystal structure
- rocksalt
- Space group
- Fm3-m
Superconducting parameters
- Hc2
- 5.1 T (0 K)
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Doping level
- 0.160