Tc max
9.0 K
Tc ambient
9.0 K
arXiv year
2011
Papers
6
Tc exp.
9.0 K
Tc theo.
—
Evidence
experimental
Tc max measured at single_crystal, ARPES, DOI: 10.1103/PhysRevB.88.220508, confirmed by 2 papers
Evidence (7 records from 6 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 9.0 | — | single_crystal | ARPES | unknown | 2013 | T1 | DOI: 10.1103/PhysRevB.88.220508 |
| 9.0 | — | — | ARPES | — | 2013 | T1 | 1308.3888 |
| 8.0 | — | polycrystal | susceptibility | — | 2014 | T1 | DOI: 10.1103/PhysRevB.89.020502 |
| 7.0 | ambient | polycrystal | susceptibility | — | 2013 | T1 | DOI: 10.1103/PhysRevB.87.100509 |
| 7.0 | — | — | neutron | s_pm | 2011 | T1 | 1106.0771 |
| — | ambient | polycrystal | specific_heat | — | 2013 | T1 | 1303.2010 |
| — | — | polycrystal | susceptibility | — | 2013 | T1 | 1303.2010 |
Superconducting parameters
- Gap structure
- nodal
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- polycrystal
- Doping type
- hole
- Doping level
- 0.900