Tc max
20.2 K
Tc ambient
10.0 K
arXiv year
2013
Papers
4
Tc exp.
20.2 K
Tc theo.
—
Evidence
experimental
Tc max measured at single_crystal, resistivity, arXiv:2305.13217, confirmed by 3 papers
Evidence (6 records from 4 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 20.2 | — | single_crystal | resistivity | — | 2023 | T1 | 2305.13217 |
| 19.3 | — | single_crystal | resistivity | — | 2023 | T1 | 2305.13217 |
| 11.0 | — | polycrystal | susceptibility | — | 2014 | T1 | DOI: 10.1103/PhysRevB.89.020502 |
| 10.0 | ambient | polycrystal | susceptibility, specific_heat | — | 2013 | T1 | DOI: 10.1103/PhysRevB.87.100509 |
| — | ambient | polycrystal | specific_heat | — | 2013 | T1 | 1303.2010 |
| — | — | polycrystal | susceptibility | — | 2013 | T1 | 1303.2010 |
Superconducting parameters
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- polycrystal
- Doping type
- hole
- Doping level
- 0.800