Tc max
28.7 K
Tc ambient
28.7 K
arXiv year
2013
Papers
1
Tc exp.
28.7 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, susceptibility, arXiv:1309.7887
Evidence (1 record from 1 paper)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 28.7 | — | polycrystal | susceptibility | — | 2013 | T2 | 1309.7887 |
Superconducting parameters
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- polycrystal
- Doping type
- hole
- Doping level
- 0.600