Tc max
5.2 K
Tc ambient
5.2 K
arXiv year
2013
Papers
3
Tc exp.
5.2 K
Tc theo.
—
Evidence
experimental
Tc max measured at ambient, polycrystal, resistivity, arXiv:1308.5930, confirmed by 3 papers
Evidence (5 records from 3 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 5.2 | ambient | polycrystal | resistivity | — | 2013 | T1 | 1308.5930 |
| 5.0 | — | polycrystal | resistivity, susceptibility | s-wave | 2013 | T1 | DOI: 10.1103/PhysRevB.88.064510 |
| 5.0 | ambient | polycrystal | susceptibility, resistivity | s-wave | 2013 | T1 | 1308.1880 |
| 4.2 | 1.6 | polycrystal | resistivity | — | 2013 | T1 | 1308.5930 |
| — | ambient | polycrystal | specific_heat | s-wave | 2013 | T1 | 1308.1880 |
Superconducting parameters
- Pairing symmetry
- s-wave
- Hc2
- 1.7 T (0 K)
- λ_eph (e–ph coupling)
- 0.68
Samples & pressure
- Sample form
- polycrystal
- Doping type
- hole
- Doping level
- 0.150