Tc max
30.0 K
Tc ambient
30.0 K
Discovery
1997
Papers
9
Tc max measured at ambient, arXiv:cond-mat/9807314, confirmed by 4 papers
Evidence (13 records from 9 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Paper |
|---|---|---|---|---|---|---|
| 35.0 | ambient | — | — | — | 2003 | cond-mat/0302329 |
| 30.0 | ambient | single_crystal | susceptibility | — | 2003 | cond-mat/0302329 |
| 30.0 | ambient | — | — | — | 2000 | cond-mat/0003504 |
| 30.0 | ambient | single_crystal | — | — | 1999 | cond-mat/9903261 |
| 30.0 | ambient | — | — | s-wave | 1998 | cond-mat/9807314 |
| 29.0 | ambient | single_crystal | susceptibility | s-wave | 2002 | cond-mat/0206432 |
| 27.0 | ambient | single_crystal | susceptibility | — | 2003 | cond-mat/0302329 |
| 25.0 | ambient | thin_film | STM, susceptibility | — | 2001 | cond-mat/0107343 |
| 24.5 | ambient | polycrystal | STM | — | 1997 | cond-mat/9710189 |
| 23.0 | ambient | single_crystal | resistivity | — | 2000 | cond-mat/0002241 |
| — | ambient | single_crystal | susceptibility | — | 2001 | cond-mat/0107343 |
| — | ambient | single_crystal | STM | — | 2000 | cond-mat/0002241 |
| — | ambient | single_crystal | susceptibility, specific_heat | — | 1999 | cond-mat/9912164 |
Structure
- Crystal structure
- cubic
- Space group
- P4mm
Superconducting parameters
- Pairing symmetry
- s-wave
- Hc2
- 5.0 T (at 22 K)
- λ_eph (e–ph coupling)
- 0.98
- ω_log
- 174 K
Competing orders
- Competing order
- CDW
Samples & pressure
- Sample form
- single_crystal
- Substrate
- (100)SrTiO_3
- Pressure type
- none
- Doping type
- hole
- Doping level
- 0.400