Tc max
5.5 K
Tc ambient
5.5 K
arXiv year
2012
Papers
3
Tc exp.
5.5 K
Tc theo.
—
Evidence
experimental
Tc max measured at resistivity, arXiv:1209.5447, confirmed by 3 papers
Evidence (4 records from 3 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 5.5 | — | — | resistivity, susceptibility, specific_heat | — | 2012 | T1 | 1209.5447 |
| 5.1 | — | polycrystal | susceptibility | — | 2013 | T1 | DOI: 10.1103/PhysRevB.88.140501 |
| 4.5 | — | polycrystal | muSR | s-wave | 2013 | T1 | DOI: 10.1103/PhysRevB.88.140501 |
| 4.2 | — | polycrystal | specific_heat | s-wave | 2013 | T1 | DOI: 10.1103/PhysRevB.88.064510 |
Structure
- Crystal structure
- tetragonal CeCr2Si2C structure
- Space group
- P4/mmm
- Lattice a (Å)
- 4.120
- Lattice c (Å)
- 8.095
Superconducting parameters
- Pairing symmetry
- s-wave
- Gap structure
- full_gap
- λ_eph (e–ph coupling)
- 0.68
Samples & pressure
- Sample form
- polycrystal
- Doping level
- 0.250