Tc max
29.0 K
Tc ambient
29.0 K
arXiv year
2010
Papers
1
Tc max measured at polycrystal, susceptibility, arXiv:1005.1411
Evidence (1 record from 1 paper)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 29.0 | — | polycrystal | susceptibility | — | 2010 | — | 1005.1411 |
Structure
- Space group
- I4/mmm
- Phase
- 122
Superconducting parameters
- λ_eph (e–ph coupling)
- —
Competing orders
- Competing order
- SDW
Samples & pressure
- Sample form
- polycrystal
- Doping type
- isovalent
- Doping level
- 0.400