Tc max
31.0 K
Tc ambient
30.0 K
arXiv year
2009
Papers
13
Tc exp.
31.0 K
Tc theo.
—
Evidence
experimental
Tc max measured at single_crystal, DOI: 10.1103/PhysRevB.84.060507, confirmed by 2 papers
Evidence (14 records from 13 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 31.0 | — | single_crystal | — | unknown | 2011 | T1 | DOI: 10.1103/PhysRevB.84.060507 |
| 31.0 | — | single_crystal | — | — | 2011 | T1 | 1103.0885 |
| 30.0 | — | single_crystal | resistivity | — | 2014 | T1 | DOI: 10.1103/PhysRevB.90.014503 |
| 30.0 | — | — | resistivity | — | 2012 | T1 | 1207.1045 |
| 30.0 | — | single_crystal | resistivity | unknown | 2012 | T1 | DOI: 10.1103/PhysRevLett.109.027006 |
| 30.0 | — | — | susceptibility | — | 2012 | T2 | 1203.1459 |
| 30.0 | — | polycrystal | susceptibility | unknown | 2010 | T1 | DOI: 10.1103/PhysRevB.81.020503 |
| 30.0 | — | single_crystal | resistivity, specific_heat | unknown | 2010 | T1 | DOI: 10.1103/PhysRevB.81.220501 |
| 30.0 | — | polycrystal | NMR, susceptibility | — | 2009 | T1 | 0908.0625 |
| 30.0 | — | single_crystal | penetration_depth, thermal_conductivity, resistivity, specific_heat | — | 2009 | T1 | 0907.4399 |
| 30.0 | — | single_crystal | — | — | 2009 | T1 | 0910.3634 |
| 27.6 | — | — | — | — | 2020 | T1 | 2007.08858 |
| — | — | single_crystal | susceptibility | — | 2020 | T1 | 2006.06789 |
| — | — | — | resistivity | — | 2009 | T1 | 0910.3634 |
Superconducting parameters
- Gap structure
- nodal
- Hc2
- 52.0 T (0 K)
- λ_eph (e–ph coupling)
- —
Competing orders
- ρ(T) exponent
- 1.00
Samples & pressure
- Sample form
- single_crystal
- Doping type
- isovalent
- Doping level
- 0.330