Tc max
20.3 K
Tc ambient
20.1 K
arXiv year
2011
Papers
14
Tc exp.
20.3 K
Tc theo.
—
Evidence
experimental
Tc max measured at single_crystal, resistivity, DOI: 10.1103/PhysRevB.92.174509, confirmed by 2 papers
Evidence (28 records from 14 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 20.5 | — | single_crystal | susceptibility | — | 2011 | T1 | DOI: 10.1103/PhysRevB.83.224522 |
| 20.3 | — | single_crystal | resistivity | — | 2015 | T1 | DOI: 10.1103/PhysRevB.92.174509 |
| 20.1 | — | single_crystal | susceptibility, resistivity | — | 2014 | — | 1409.6402 |
| 20.0 | — | single_crystal | resistivity | — | 2017 | T1 | 1703.07730 |
| 20.0 | ambient | single_crystal | susceptibility | s-wave | 2015 | T1 | DOI: 10.1103/PhysRevB.91.024510 |
| 19.9 | — | single_crystal | resistivity | — | 2015 | T1 | DOI: 10.1103/PhysRevB.92.174509 |
| 19.0 | ambient | single_crystal | susceptibility | s-wave | 2015 | T1 | DOI: 10.1103/PhysRevB.91.024510 |
| 19.0 | — | single_crystal | neutron | — | 2014 | T1 | DOI: 10.1103/PhysRevB.90.024509 |
| 19.0 | — | single_crystal | neutron | — | 2012 | T1 | DOI: 10.1103/PhysRevLett.108.247002 |
| 18.6 | — | single_crystal | resistivity | — | 2015 | T1 | DOI: 10.1103/PhysRevB.92.174509 |
| 18.5 | — | single_crystal | susceptibility, Andreev spectroscopy | unknown | 2016 | T1 | 1608.01649 |
| 18.5 | ambient | single_crystal | susceptibility | s-wave | 2015 | T1 | DOI: 10.1103/PhysRevB.91.024510 |
| 18.2 | — | single_crystal | resistivity | — | 2015 | T1 | DOI: 10.1103/PhysRevB.92.174509 |
| 15.0 | — | single_crystal | neutron | — | 2012 | T1 | DOI: 10.1103/PhysRevLett.108.247002 |
| 14.5 | — | single_crystal | resistivity | — | 2015 | T1 | DOI: 10.1103/PhysRevB.92.174509 |
| 13.9 | ambient | single_crystal | susceptibility | s-wave | 2015 | T1 | DOI: 10.1103/PhysRevB.91.024510 |
| 13.7 | — | single_crystal | resistivity | — | 2015 | T1 | DOI: 10.1103/PhysRevB.92.174509 |
| 11.5 | — | single_crystal | susceptibility | — | 2011 | T1 | DOI: 10.1103/PhysRevB.83.224522 |
| 11.3 | — | single_crystal | resistivity | — | 2015 | T1 | DOI: 10.1103/PhysRevB.92.174509 |
| 10.9 | — | single_crystal | resistivity | — | 2015 | T1 | DOI: 10.1103/PhysRevB.92.174509 |
| 7.7 | ambient | single_crystal | susceptibility | s-wave | 2015 | T1 | DOI: 10.1103/PhysRevB.91.024510 |
| 3.4 | — | single_crystal | resistivity | — | 2015 | T1 | DOI: 10.1103/PhysRevB.92.174509 |
| — | — | single_crystal | resistivity | — | 2019 | T1 | DOI: 10.1103/PhysRevResearch.1.033154 |
| — | — | single_crystal | resistivity | — | 2018 | T1 | 1803.11149 |
| — | — | single_crystal | resistivity | — | 2017 | T1 | DOI: 10.1103/PhysRevLett.119.157001 |
| — | — | single_crystal | specific_heat | — | 2016 | T1 | 1605.04669 |
| — | — | single_crystal | specific_heat, susceptibility | unknown | 2015 | — | 1502.07130 |
| — | — | — | resistivity | — | 2014 | T1 | 1406.5829 |
Structure
- Crystal structure
- orthorhombic
- Lattice a (Å)
- 5.600
- Lattice c (Å)
- 12.900
Superconducting parameters
- Gap structure
- multi_gap
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- single_crystal
- Pressure type
- none
- Doping type
- electron
- Doping level
- 0.100