Tc max
5.3 K
Tc ambient
5.3 K
arXiv year
2007
Papers
7
Tc exp.
5.3 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, specific_heat, arXiv:0710.0738, confirmed by 2 papers
Evidence (10 records from 7 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 5.3 | — | polycrystal | specific_heat | s-wave | 2007 | T1 | 0710.0738 |
| 5.3 | ambient | polycrystal | specific_heat | s-wave | 2007 | T1 | DOI: 10.1103/PhysRevLett.99.217001 |
| 5.3 | — | polycrystal | resistivity | — | 2007 | T1 | 0710.0738 |
| 5.3 | ambient | polycrystal | resistivity, susceptibility | s-wave | 2007 | T1 | DOI: 10.1103/PhysRevLett.99.217001 |
| 5.0 | — | polycrystal | susceptibility, specific_heat | — | 2008 | T1 | DOI: 10.1103/PhysRevB.78.052504 |
| 5.0 | ambient | — | specific_heat | — | 2007 | T1 | 0710.1413 |
| 5.0 | — | polycrystal | susceptibility | — | 2008 | T1 | DOI: 10.1103/PhysRevLett.100.017002 |
| 5.0 | ambient | — | susceptibility | — | 2007 | T1 | 0710.1413 |
| 4.9 | — | polycrystal | susceptibility, muSR, specific_heat, resistivity | s-wave | 2012 | T1 | 1211.4222 |
| 4.9 | — | polycrystal | susceptibility, muSR | s-wave | 2012 | T1 | DOI: 10.1103/PhysRevB.86.174513 |
Structure
- Crystal structure
- skutterudite
- Space group
- Im-3 (#204)
- Lattice a (Å)
- 8.693
Superconducting parameters
- Pairing symmetry
- s-wave
- Gap structure
- full_gap
- Hc2
- 1.8 T (0 K)
- λ_eph (e–ph coupling)
- 0.70
Samples & pressure
- Sample form
- polycrystal
- Pressure type
- none
- Doping type
- none
- Doping level
- 0.000