Tc max
85.7 K
Tc ambient
85.7 K
Discovery
2003
Papers
2
Tc max measured at ambient, single_crystal, specific_heat, arXiv:cond-mat/0302024, confirmed by 2 papers
Evidence (2 records from 2 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Paper |
|---|---|---|---|---|---|---|
| 85.7 | ambient | single_crystal | specific_heat | — | 2003 | cond-mat/0302024 |
| 85.7 | ambient | — | specific_heat | — | 2003 | cond-mat/0306668 |
Superconducting parameters
- λ_eph (e–ph coupling)
- —