Tc max
20.0 K
Tc ambient
20.0 K
arXiv year
2016
Papers
1
Tc max measured at single_crystal, resistivity, arXiv:1603.04899
Evidence (2 records from 1 paper)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 20.0 | — | single_crystal | resistivity | — | 2016 | — | 1603.04899 |
| 16.0 | — | single_crystal | specific_heat | s_pm | 2016 | — | 1603.04899 |
Superconducting parameters
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Doping level
- 0.046