Tc max
20.7 K
Tc ambient
20.4 K
arXiv year
2010
Papers
1
Tc exp.
20.7 K
Tc theo.
—
Evidence
experimental
Tc max measured at P=0.4 GPa, polycrystal, resistivity, DOI: 10.1103/PhysRevB.81.054507
Evidence (2 records from 1 paper)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 20.7 | 0.4 | polycrystal | resistivity | — | 2010 | T1 | DOI: 10.1103/PhysRevB.81.054507 |
| 20.4 | ambient | polycrystal | resistivity | — | 2010 | T1 | DOI: 10.1103/PhysRevB.81.054507 |
Structure
- Crystal structure
- ZrCuSiAs-type
Superconducting parameters
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Doping level
- 0.150