Tc max
81.0 K
Tc ambient
—
arXiv year
1993
Papers
16
Tc exp.
81.0 K
Tc theo.
82.3 K
Evidence
experimental
Tc max measured at polycrystal, susceptibility, DOI: 10.1103/PhysRevB.82.172509, confirmed by 2 papers
Evidence (19 records from 16 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 82.3 | — | — | — | — | 2012 | T1 | 1211.1298 |
| 82.3 | — | — | — | — | 2012 | T1 | DOI: 10.1103/PhysRevB.86.144533 |
| 81.5 | — | polycrystal | resistivity | — | 1995 | T1 | DOI: 10.1103/PhysRevB.51.6739 |
| 81.0 | — | polycrystal | susceptibility | — | 2010 | T1 | DOI: 10.1103/PhysRevB.82.172509 |
| 80.5 | — | — | — | — | 2012 | T1 | 1211.1298 |
| 80.0 | — | polycrystal | — | — | 1993 | T1 | DOI: 10.1103/PhysRevB.48.532 |
| 78.0 | — | single_crystal | susceptibility | — | 2015 | T1 | DOI: 10.1103/PhysRevB.92.104507 |
| 57.0 | — | polycrystal | susceptibility | — | 2010 | T1 | DOI: 10.1103/PhysRevB.82.172509 |
| 46.0 | — | single_crystal | susceptibility | — | 2015 | T1 | DOI: 10.1103/PhysRevB.92.104507 |
| 33.1 | — | polycrystal | resistivity | — | 2002 | T1 | DOI: 10.1103/PhysRevLett.88.137003 |
| — | — | single_crystal | susceptibility | — | 2019 | T1 | DOI: 10.1103/PhysRevB.100.035129 |
| — | — | — | — | — | 2014 | T1 | 1403.5574 |
| — | — | single_crystal | susceptibility | — | 2014 | T1 | DOI: 10.1103/PhysRevB.90.104511 |
| — | — | — | resistivity | — | 2009 | T1 | 0909.1040 |
| — | — | polycrystal | resistivity | — | 2008 | T1 | DOI: 10.1103/PhysRevB.78.140508 |
| — | — | polycrystal | resistivity | — | 2008 | T1 | DOI: 10.1103/PhysRevB.78.020505 |
| — | — | — | resistivity, muSR | — | 2002 | T1 | cond-mat/0211405 |
| — | — | polycrystal | resistivity | — | 1998 | T1 | DOI: 10.1103/PhysRevB.58.11204 |
| — | — | polycrystal | — | — | 1996 | T1 | DOI: 10.1103/PhysRevB.53.14631 |
Structure
- Crystal structure
- tetragonal
- Space group
- P4/mmm (#123)
Superconducting parameters
- Pairing symmetry
- d-wave
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- polycrystal
- Doping level
- 0.250