Tc max
0.5 K
Tc ambient
0.5 K
arXiv year
1999
Papers
5
Tc exp.
0.5 K
Tc theo.
1.0 K
Evidence
mixed
Tc max measured at polycrystal, susceptibility, DOI: 10.1103/PhysRevLett.94.207002, confirmed by 2 papers
Evidence (5 records from 5 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 1.0 | — | — | — | — | 2010 | T2 | 1008.2822 |
| 0.5 | — | polycrystal | susceptibility | s-wave | 2005 | T1 | DOI: 10.1103/PhysRevLett.94.207002 |
| 0.5 | — | polycrystal | susceptibility | s-wave | 2003 | T1 | DOI: 10.1103/PhysRevB.67.012506 |
| — | — | thin_film | — | — | 2007 | T1 | DOI: 10.1103/PhysRevB.75.014519 |
| — | — | — | resistivity | — | 1999 | T2 | cond-mat/9905294 |
Superconducting parameters
- Pairing symmetry
- s-wave
- Gap structure
- full_gap
- λ_eph (e–ph coupling)
- 0.55
Samples & pressure
- Sample form
- polycrystal