Tc max
0.7 K
Tc ambient
0.7 K
arXiv year
2009
Papers
13
Tc exp.
0.7 K
Tc theo.
—
Evidence
experimental
Tc max measured at ambient, single_crystal, resistivity, DOI: 10.1103/PhysRevLett.104.059701, confirmed by 5 papers
Evidence (14 records from 13 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 0.7 | ambient | polycrystal | resistivity | — | 2011 | T1 | DOI: 10.1103/PhysRevB.83.064504 |
| 0.7 | ambient | single_crystal | resistivity | — | 2010 | T1 | DOI: 10.1103/PhysRevLett.104.059701 |
| 0.7 | — | single_crystal | resistivity, specific_heat, susceptibility | — | 2010 | T1 | 1001.4397 |
| 0.7 | ambient | polycrystal | resistivity, specific_heat | — | 2010 | T1 | 1001.4607 |
| 0.7 | — | single_crystal | resistivity, specific_heat | — | 2010 | T1 | 1001.4609 |
| 0.7 | — | single_crystal | resistivity | — | 2010 | T1 | 1001.4403 |
| 0.7 | ambient | polycrystal | muSR | d-wave | 2012 | T1 | DOI: 10.1103/PhysRevB.86.094525 |
| 0.7 | ambient | single_crystal | resistivity, susceptibility | unknown | 2011 | T1 | DOI: 10.1103/PhysRevX.1.011010 |
| 0.7 | ambient | single_crystal | resistivity, specific_heat | — | 2009 | T1 | DOI: 10.1103/PhysRevLett.103.027003 |
| 0.7 | ambient | single_crystal | resistivity, specific_heat | — | 2009 | T1 | 0906.1881 |
| 0.6 | — | polycrystal | susceptibility | d-wave | 2012 | — | 1209.2765 |
| 0.6 | — | polycrystal | susceptibility | d-wave | 2012 | T1 | DOI: 10.1103/PhysRevB.86.094508 |
| 0.5 | ambient | single_crystal | resistivity | — | 2010 | T1 | DOI: 10.1103/PhysRevLett.104.059701 |
| — | — | — | resistivity | — | 2010 | T1 | 1008.0679 |
Structure
- Crystal structure
- Ho2CoGa8-type
- Space group
- P4/mmm
Superconducting parameters
- Pairing symmetry
- d-wave
- Gap structure
- nodal
- Hc2
- 4.8 T (0 K)
- λ_eph (e–ph coupling)
- —
Competing orders
- Competing order
- AFM
- T_AFM
- 10.0 K
- ρ(T) exponent
- 1.00
Samples & pressure
- Sample form
- single_crystal
- Pressure type
- none