Tc max
0.4 K
Tc ambient
0.4 K
Discovery
2000
Papers
5
Tc max measured at P=0.19 GPa, polycrystal, arXiv:cond-mat/0311296, confirmed by 4 papers
Evidence (10 records from 5 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Paper |
|---|---|---|---|---|---|---|
| 0.5 | 0.6 | — | NQR | — | 2004 | cond-mat/0405348 |
| 0.5 | 0.9 | — | NQR | — | 2004 | cond-mat/0405348 |
| 0.5 | 0.2 | polycrystal | — | — | 2003 | cond-mat/0311296 |
| 0.5 | 0.6 | polycrystal | — | — | 2003 | cond-mat/0311296 |
| 0.5 | 0.9 | polycrystal | — | — | 2003 | cond-mat/0311296 |
| 0.4 | ambient | — | NQR | — | 2004 | cond-mat/0405348 |
| 0.4 | ambient | polycrystal | — | — | 2003 | cond-mat/0311296 |
| 0.4 | ambient | — | NQR | — | 2002 | cond-mat/0201040 |
| 0.4 | ambient | polycrystal | susceptibility | — | 2000 | cond-mat/0012154 |
| — | — | — | muSR | d-wave | 2003 | cond-mat/0306456 |
Superconducting parameters
- Gap structure
- nodal
- λ_eph (e–ph coupling)
- —
Competing orders
- Competing order
- AFM
- T_AFM
- 0.8 K
Samples & pressure
- Sample form
- polycrystal
- Pressure type
- hydrostatic
- Doping type
- isovalent
- Doping level
- 0.020