Tc max
9.1 K
Tc ambient
9.1 K
Discovery
2004
Papers
1
Tc max measured at ambient, powder, susceptibility, arXiv:cond-mat/0402501
Evidence (1 record from 1 paper)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Paper |
|---|---|---|---|---|---|---|
| 9.1 | ambient | powder | susceptibility | — | 2004 | cond-mat/0402501 |
Structure
- Crystal structure
- 3R-type
- Lattice a (Å)
- 5.720
Superconducting parameters
- λ_eph (e–ph coupling)
- —
Competing orders
- Competing order
- AFM
- T_AFM
- 18.6 K
Samples & pressure
- Sample form
- powder
- Doping level
- 0.330