Tc max
6.4 K
Tc ambient
4.7 K
Discovery
2002
Papers
1
Tc max measured at P=4 GPa, polycrystal, resistivity, arXiv:cond-mat/0211232
Evidence (2 records from 1 paper)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Paper |
|---|---|---|---|---|---|---|
| 6.4 | 4.0 | polycrystal | resistivity | — | 2002 | cond-mat/0211232 |
| 4.7 | ambient | polycrystal | resistivity | — | 2002 | cond-mat/0211232 |
Structure
- Crystal structure
- spinel
- Lattice a (Å)
- 9.787
Superconducting parameters
- λ_eph (e–ph coupling)
- —