SCLib
JZIS
Home
Search
Materials
Timeline
Discovery
Stats
Account
← Materials
Eu
0.73
La
0.27
Fe
2
As
2
…
iron_based
unconventional
Tc max
—
Tc ambient
—
arXiv year
2012
Papers
1
Evidence (2 records from 1 paper)
the flat columns above are aggregates — each line here is one paper's claim
Tc (K)
P (GPa)
Sample
Method
Pairing
Year
Tier
Paper
—
ambient
—
resistivity
—
2012
T1
1201.1706
↗
—
0.5
—
resistivity
—
2012
T1
1201.1706
↗
Superconducting parameters
λ_eph (e–ph coupling)
—
Samples & pressure
Doping level
0.270