Tc max
2.3 K
Tc ambient
—
arXiv year
2005
Papers
6
Tc exp.
2.3 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, resistivity, DOI: 10.1103/PhysRevB.74.174509
Evidence (6 records from 6 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 2.3 | — | polycrystal | resistivity | — | 2006 | T1 | DOI: 10.1103/PhysRevB.74.174509 |
| — | — | — | resistivity | — | 2009 | T1 | 0904.3499 |
| — | — | polycrystal | susceptibility | — | 2009 | T1 | DOI: 10.1103/PhysRevB.79.184524 |
| — | — | polycrystal | resistivity | — | 2009 | T1 | DOI: 10.1103/PhysRevB.79.184525 |
| — | — | — | susceptibility | — | 2008 | T1 | 0811.2913 |
| — | — | — | resistivity | — | 2005 | T2 | cond-mat/0510616 |
Superconducting parameters
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- polycrystal