Tc max
8.9 K
Tc ambient
8.9 K
arXiv year
2014
Papers
1
Tc exp.
8.9 K
Tc theo.
—
Evidence
experimental
Tc max measured at single_crystal, resistivity, arXiv:1411.3664
Evidence (1 record from 1 paper)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 8.9 | — | single_crystal | resistivity | — | 2014 | T1 | 1411.3664 |
Structure
- Crystal structure
- tetragonal
- Lattice a (Å)
- 3.770
- Lattice c (Å)
- 5.520
Superconducting parameters
- Gap structure
- multi_gap
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- single_crystal
- Pressure type
- none
- Doping type
- none
- Doping level
- 0.040