Tc max
8.7 K
Tc ambient
8.0 K
arXiv year
2009
Papers
5
Tc exp.
8.7 K
Tc theo.
—
Evidence
experimental
Tc max measured at single_crystal, resistivity, arXiv:0908.3011, confirmed by 2 papers
Evidence (8 records from 5 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 8.7 | — | single_crystal | resistivity, susceptibility | — | 2009 | — | 0908.3011 |
| 8.7 | — | single_crystal | resistivity | — | 2009 | T1 | DOI: 10.1103/PhysRevB.80.214514 |
| 8.0 | — | single_crystal | resistivity | — | 2010 | T1 | DOI: 10.1103/PhysRevB.81.174518 |
| 8.0 | — | — | — | — | 2010 | T1 | 1002.1948 |
| 8.0 | — | single_crystal | susceptibility | s-wave | 2010 | — | 1001.2042 |
| 7.5 | — | single_crystal | susceptibility | s-wave | 2010 | — | 1001.2042 |
| 7.0 | — | single_crystal | resistivity | — | 2009 | — | 0908.3011 |
| 7.0 | — | single_crystal | resistivity | — | 2009 | T1 | DOI: 10.1103/PhysRevB.80.214514 |
Structure
- Crystal structure
- P4/nmm
- Space group
- P4/nmm
Superconducting parameters
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- single_crystal