Tc max
2.4 K
Tc ambient
2.4 K
arXiv year
2003
Papers
5
Tc exp.
2.4 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, resistivity, arXiv:cond-mat/0611393, confirmed by 2 papers
Evidence (5 records from 5 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 2.4 | — | polycrystal | resistivity | — | 2006 | T2 | cond-mat/0611393 |
| 2.3 | ambient | polycrystal | resistivity | — | 2003 | T1 | DOI: 10.1103/PhysRevLett.91.127004 |
| — | — | polycrystal | — | — | 2008 | — | 0807.2788 |
| — | — | — | resistivity, susceptibility | — | 2008 | — | 0812.1003 |
| — | — | — | susceptibility | — | 2008 | T1 | 0811.2913 |
Superconducting parameters
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- polycrystal
- Doping level
- 0.300