Tc max
8.0 K
Tc ambient
—
arXiv year
2017
Papers
4
Tc exp.
8.0 K
Tc theo.
—
Evidence
experimental
Tc max measured at P=30 GPa, polycrystal, resistivity, arXiv:1605.01757, confirmed by 3 papers
Evidence (8 records from 4 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 8.0 | 30.0 | polycrystal | resistivity | — | 2017 | — | 1605.01757 |
| 8.0 | 30.0 | powder | resistivity | — | 2017 | T1 | DOI: 10.1103/PhysRevB.95.064514 |
| 6.6 | 27.0 | polycrystal | resistivity | — | 2018 | T1 | DOI: 10.1103/PhysRevB.97.024513 |
| 6.0 | 20.0 | polycrystal | resistivity | — | 2017 | — | 1605.01757 |
| 6.0 | 20.0 | powder | resistivity | — | 2017 | T1 | DOI: 10.1103/PhysRevB.95.064514 |
| 5.8 | 10.4 | polycrystal | resistivity | — | 2018 | T1 | DOI: 10.1103/PhysRevB.97.024513 |
| 1.8 | 4.0 | polycrystal | resistivity | — | 2018 | T1 | DOI: 10.1103/PhysRevB.97.024513 |
| — | — | — | — | — | 2017 | T1 | 1709.01844 |
Structure
- Crystal structure
- fcc
Superconducting parameters
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- polycrystal
- Pressure type
- hydrostatic