Tc max
132.0 K
Tc ambient
132.0 K
arXiv year
1998
Papers
1
Tc exp.
132.0 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, susceptibility, DOI: 10.1103/PhysRevB.57.1259
Evidence (3 records from 1 paper)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 132.0 | — | polycrystal | susceptibility | — | 1998 | T1 | DOI: 10.1103/PhysRevB.57.1259 |
| 128.0 | — | polycrystal | susceptibility | — | 1998 | T1 | DOI: 10.1103/PhysRevB.57.1259 |
| 120.0 | — | polycrystal | susceptibility | — | 1998 | T1 | DOI: 10.1103/PhysRevB.57.1259 |
Structure
- Crystal structure
- tetragonal
- Space group
- P4/mmm
- Lattice a (Å)
- 3.865
- Lattice c (Å)
- 15.957
Superconducting parameters
- Pairing symmetry
- d-wave
- λ_eph (e–ph coupling)
- —