Tc max
8.7 K
Tc ambient
8.7 K
Discovery
1995
Papers
5
Tc max measured at ambient, resistivity, arXiv:cond-mat/0008030, confirmed by 4 papers
Evidence (6 records from 5 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Paper |
|---|---|---|---|---|---|---|
| 8.7 | ambient | — | resistivity | unknown | 2000 | cond-mat/0008030 |
| 8.0 | ambient | single_crystal | specific_heat | — | 2003 | cond-mat/0307041 |
| 8.0 | ambient | polycrystal | neutron | — | 1995 | supr-con/9505002 |
| 8.0 | ambient | single_crystal | resistivity | — | 1995 | supr-con/9504001 |
| 6.6 | ambient | — | resistivity | s-wave | 2000 | cond-mat/0008030 |
| — | ambient | single_crystal | thermal conductivity, resistivity | — | 2003 | cond-mat/0301207 |
Structure
- Crystal structure
- body-centered tetragonal
- Space group
- I4/mmm (#139)
- Lattice a (Å)
- 3.517
- Lattice c (Å)
- 10.522
Superconducting parameters
- λ_eph (e–ph coupling)
- —
Competing orders
- T_SDW
- 8.5 K
- T_AFM
- 8.0 K
Samples & pressure
- Sample form
- single_crystal
- Pressure type
- none