Tc max
10.0 K
Tc ambient
9.7 K
arXiv year
2004
Papers
33
Tc exp.
10.0 K
Tc theo.
9.6 K
Evidence
experimental
Tc max measured at P=0.35 GPa, susceptibility, arXiv:0802.1179, confirmed by 3 papers
Evidence (43 records from 33 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 10.0 | 0.3 | — | susceptibility | s-wave | 2008 | T1 | 0802.1179 |
| 10.0 | 0.5 | — | susceptibility | s-wave | 2008 | T1 | 0802.1179 |
| 10.0 | 0.6 | polycrystal | resistivity | — | 2005 | T1 | DOI: 10.1103/PhysRevLett.95.167004 |
| 10.0 | 0.6 | — | resistivity | — | 2005 | T1 | cond-mat/0502490 |
| 9.7 | — | polycrystal | susceptibility | — | 2011 | T1 | DOI: 10.1103/PhysRevB.83.104503 |
| 9.7 | ambient | polycrystal | resistivity, susceptibility, specific_heat | — | 2011 | T1 | 1101.3639 |
| 9.7 | 1.0 | single_crystal | resistivity | — | 2010 | T1 | 1009.0355 |
| 9.7 | — | polycrystal | susceptibility | s-wave | 2007 | T1 | DOI: 10.1103/PhysRevLett.98.227003 |
| 9.7 | — | single_crystal | resistivity, susceptibility | — | 2006 | T1 | DOI: 10.1103/PhysRevB.73.144506 |
| 9.7 | — | single_crystal | resistivity | unknown | 2006 | — | cond-mat/0601465 |
| 9.6 | ambient | — | susceptibility | s-wave | 2008 | T1 | 0802.1179 |
| 9.6 | — | single_crystal | susceptibility, STM | s-wave | 2008 | T1 | DOI: 10.1103/PhysRevLett.101.057004 |
| 9.6 | ambient | single_crystal | specific_heat, resistivity | s-wave | 2007 | T1 | DOI: 10.1103/PhysRevB.76.014523 |
| 9.6 | — | powder | muSR | — | 2007 | T1 | DOI: 10.1103/PhysRevLett.98.197002 |
| 9.6 | — | single_crystal | ARPES | s-wave | 2007 | T1 | DOI: 10.1103/PhysRevLett.99.117003 |
| 9.6 | — | single_crystal | susceptibility | — | 2007 | T1 | DOI: 10.1103/PhysRevLett.99.257001 |
| 9.6 | — | single_crystal | STM, susceptibility | s-wave | 2007 | T1 | 0704.0529 |
| 9.6 | — | single_crystal | — | s-wave | 2006 | T1 | DOI: 10.1103/PhysRevLett.96.247004 |
| 9.6 | — | single_crystal | resistivity, susceptibility | s-wave | 2006 | — | cond-mat/0603309 |
| 9.6 | — | — | resistivity | — | 2006 | T1 | cond-mat/0607064 |
| 9.6 | — | single_crystal | resistivity, susceptibility | s-wave | 2006 | T1 | DOI: 10.1103/PhysRevB.74.220506 |
| 9.6 | — | single_crystal | thermal_conductivity | — | 2006 | T2 | cond-mat/0603036 |
| 9.6 | — | single_crystal | resistivity | — | 2006 | T1 | cond-mat/0602433 |
| 9.6 | — | powder | NMR | — | 2006 | — | cond-mat/0610760 |
| 9.6 | ambient | polycrystal | resistivity | — | 2005 | T1 | DOI: 10.1103/PhysRevLett.95.167004 |
| 9.6 | — | — | — | — | 2004 | T2 | cond-mat/0406538 |
| 9.5 | — | single_crystal | susceptibility | s-wave | 2007 | T1 | DOI: 10.1103/PhysRevLett.98.257004 |
| 9.5 | — | single_crystal | specific_heat | unknown | 2006 | T1 | DOI: 10.1103/PhysRevB.73.094518 |
| 9.4 | 1.1 | — | susceptibility | s-wave | 2008 | T1 | 0802.1179 |
| 9.0 | — | single_crystal | susceptibility | s-wave | 2007 | T1 | 0705.2615 |
| 9.0 | — | polycrystal | muSR | unknown | 2004 | T2 | cond-mat/0402400 |
| 8.9 | — | polycrystal | muSR | unknown | 2004 | T2 | cond-mat/0402400 |
| 8.3 | — | — | — | — | 2018 | T1 | 1807.04658 |
| 6.5 | 3.5 | single_crystal | resistivity | — | 2010 | T1 | 1009.0355 |
| 6.0 | — | — | — | — | 2018 | T1 | 1807.04658 |
| 5.1 | — | — | — | — | 2018 | T1 | 1807.04658 |
| 3.3 | 3.6 | single_crystal | resistivity | — | 2010 | T1 | 1009.0355 |
| — | — | single_crystal | susceptibility | — | 2012 | T1 | 1201.5425 |
| — | — | single_crystal | magnetic_torque, dHvA | — | 2010 | T1 | 1005.3089 |
| — | — | single_crystal | — | s-wave | 2009 | T1 | 0906.4656 |
| — | ambient | single_crystal | resistivity | — | 2007 | T1 | 0705.1401 |
| — | 2.3 | single_crystal | resistivity | — | 2007 | T1 | 0705.1401 |
| — | — | single_crystal | specific_heat, resistivity, susceptibility | — | 2006 | T2 | cond-mat/0602579 |
Structure
- Crystal structure
- F4-3m
- Space group
- F4-3m
- Lattice a (Å)
- 10.072
Superconducting parameters
- Pairing symmetry
- s-wave
- Gap structure
- full_gap
- Hc2
- 33.0 T (0.05 K)
- λ_eph (e–ph coupling)
- 6.60
- ω_log
- 26 K
Competing orders
- T_CDW
- 7.0 K
- ρ(T) exponent
- 2.00
Samples & pressure
- Sample form
- single_crystal
- Doping type
- none