Tc max
26.5 K
Tc ambient
—
arXiv year
2012
Papers
1
Tc max measured at polycrystal, susceptibility, arXiv:1209.6512
Evidence (1 record from 1 paper)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 26.5 | — | polycrystal | susceptibility | — | 2012 | — | 1209.6512 |
Superconducting parameters
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- polycrystal