← Materials
La1.895Sr0.105CuO4
cuprate · orthorhombic · cuprate_214
ambient SCunconventionalcompeting order
Tc max
30.0 K
Tc ambient
30.0 K
arXiv year
1997
Papers
8
Tc exp.
30.0 K
Tc theo.
—
Evidence
experimental
Tc max measured at arXiv:0712.2181, confirmed by 6 papers
Evidence (8 records from 8 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 30.0 | — | single_crystal | ARPES | d-wave | 2008 | T1 | 0810.0292 |
| 30.0 | — | single_crystal | ARPES | d-wave | 2008 | T1 | DOI: 10.1103/PhysRevLett.101.047002 |
| 30.0 | — | — | — | — | 2007 | T1 | 0712.2181 |
| 30.0 | — | single_crystal | ARPES | d-wave | 2007 | T1 | 0708.2333 |
| 30.0 | — | single_crystal | specific_heat | — | 2007 | T1 | cond-mat/0701404 |
| 30.0 | — | single_crystal | specific_heat, neutron | d-wave | 2007 | T1 | DOI: 10.1103/PhysRevLett.98.077004 |
| — | — | single_crystal | neutron | — | 2012 | T1 | 1204.2152 |
| — | — | thin_film | resistivity | — | 1997 | T2 | cond-mat/9705107 |
Structure
- Crystal structure
- orthorhombic
- Phase
- cuprate_214
Superconducting parameters
- Pairing symmetry
- d-wave
- Gap structure
- nodal
- λ_eph (e–ph coupling)
- —
Competing orders
- Competing order
- AFM
Samples & pressure
- Sample form
- single_crystal
- Substrate
- LaSrAlO3
- Doping type
- hole
- Doping level
- 0.105