Tc max
20.0 K
Tc ambient
20.0 K
arXiv year
2015
Papers
3
Tc exp.
20.0 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, arXiv:1907.06211, confirmed by 2 papers
Evidence (3 records from 3 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 20.0 | — | polycrystal | — | — | 2019 | T1 | 1907.06211 |
| 15.0 | — | polycrystal | susceptibility | — | 2015 | T1 | 1512.08095 |
| — | — | polycrystal | susceptibility | d-wave | 2016 | T1 | 1607.07953 |
Structure
- Crystal structure
- Nd2CuO4-type structure
Superconducting parameters
- Pairing symmetry
- d-wave
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- polycrystal
- Doping level
- 0.000