Tc max
20.0 K
Tc ambient
20.0 K
Discovery
1999
Papers
7
Tc max measured at ambient, resistivity, arXiv:cond-mat/0406232, confirmed by 2 papers
Evidence (7 records from 7 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Paper |
|---|---|---|---|---|---|---|
| 27.0 | ambient | single_crystal | resistivity | d-wave | 2001 | cond-mat/0108277 |
| 20.0 | ambient | — | resistivity | — | 2004 | cond-mat/0406232 |
| 16.0 | ambient | single_crystal | susceptibility | — | 1999 | cond-mat/9909342 |
| 9.6 | ambient | polycrystal | Andreev reflection | s+d-wave | 2001 | cond-mat/0101209 |
| 9.6 | ambient | polycrystal | STM | s-wave | 2001 | cond-mat/0107289 |
| — | ambient | polycrystal | susceptibility | — | 2003 | cond-mat/0304482 |
| — | ambient | polycrystal | resistivity, susceptibility | — | 2002 | cond-mat/0207411 |
Structure
- Phase
- cuprate_214
Superconducting parameters
- Hc2
- 52.0 T (0 K)
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- polycrystal
- Pressure type
- none
- Doping type
- hole
- Doping level
- 0.080