Tc max
13.4 K
Tc ambient
13.4 K
arXiv year
2005
Papers
11
Tc exp.
13.4 K
Tc theo.
13.4 K
Evidence
experimental
Tc max measured at polycrystal, specific_heat, arXiv:cond-mat/0703279, confirmed by 4 papers
Evidence (14 records from 11 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 13.5 | ambient | polycrystal | resistivity, susceptibility, specific_heat | — | 2005 | T1 | DOI: 10.1103/PhysRevB.72.064520 |
| 13.4 | — | polycrystal | specific_heat | s-wave | 2007 | T2 | cond-mat/0703279 |
| 13.4 | ambient | polycrystal | specific_heat | — | 2007 | T1 | DOI: 10.1103/PhysRevB.76.014516 |
| 13.4 | — | — | resistivity | s-wave | 2007 | T2 | cond-mat/0701702 |
| 13.0 | ambient | — | resistivity, susceptibility | — | 2005 | T2 | cond-mat/0503597 |
| 12.0 | — | polycrystal | susceptibility | — | 2005 | T1 | DOI: 10.1103/PhysRevB.72.132505 |
| 11.8 | — | polycrystal | susceptibility | — | 2014 | T1 | DOI: 10.1103/PhysRevB.90.104507 |
| 11.2 | ambient | polycrystal | susceptibility | unknown | 2008 | T1 | 0801.4176 |
| 11.2 | ambient | polycrystal | susceptibility | s-wave | 2008 | T1 | DOI: 10.1103/PhysRevLett.100.097002 |
| 11.0 | ambient | polycrystal | muSR | unknown | 2008 | T1 | 0801.4176 |
| 11.0 | ambient | polycrystal | muSR | s-wave | 2008 | T1 | DOI: 10.1103/PhysRevLett.100.097002 |
| 10.9 | — | polycrystal | muSR | — | 2008 | T1 | 0809.1274 |
| 6.5 | — | single_crystal | susceptibility, ARPES | s-wave | 2007 | T1 | DOI: 10.1103/PhysRevB.76.132512 |
| 6.0 | — | — | resistivity | s-wave | 2007 | T2 | cond-mat/0701702 |
Structure
- Crystal structure
- cubic Pu2C3-type
- Space group
- I43d (No. 220)
- Lattice a (Å)
- 8.808
Superconducting parameters
- Pairing symmetry
- s-wave
- Gap structure
- multi_gap
- Hc2
- 16.7 T (0 K)
- λ_eph (e–ph coupling)
- 1.35
- ω_log
- 110 K
Samples & pressure
- Sample form
- polycrystal
- Pressure type
- none
- Doping type
- none