Tc max
4.0 K
Tc ambient
4.0 K
arXiv year
2008
Papers
3
Tc exp.
4.0 K
Tc theo.
—
Evidence
experimental
Tc max measured at ambient, polycrystal, susceptibility, arXiv:1002.1506, confirmed by 3 papers
Evidence (4 records from 3 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 4.0 | ambient | polycrystal | susceptibility | s-wave | 2010 | T1 | 1002.1506 |
| 2.8 | — | polycrystal | resistivity | — | 2008 | T1 | DOI: 10.1103/PhysRevB.78.060504 |
| 2.4 | — | polycrystal | susceptibility | s-wave | 2010 | T1 | DOI: 10.1103/PhysRevB.81.140509 |
| 1.8 | — | polycrystal | susceptibility | — | 2008 | T1 | DOI: 10.1103/PhysRevB.78.060504 |
Structure
- Crystal structure
- ZrCuSiAs-type
- Space group
- P4/nmm
- Lattice a (Å)
- 4.119
- Lattice c (Å)
- 8.180
Superconducting parameters
- Pairing symmetry
- s-wave
- Gap structure
- full_gap
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- polycrystal
- Doping type
- none
- Doping level
- 0.000