Tc max
11.0 K
Tc ambient
10.5 K
arXiv year
1994
Papers
6
Tc exp.
11.0 K
Tc theo.
10.4 K
Evidence
mixed
Tc max measured at polycrystal, susceptibility, DOI: 10.1103/PhysRevB.53.3492
Evidence (7 records from 6 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 11.0 | — | polycrystal | susceptibility | — | 1996 | T1 | DOI: 10.1103/PhysRevB.53.3492 |
| 10.5 | — | polycrystal | susceptibility | — | 2002 | T1 | DOI: 10.1103/PhysRevB.65.132519 |
| 10.5 |
Structure
- Crystal structure
- I4/mmm
- Space group
- I4/mmm
- Lattice a (Å)
- 3.904
- Lattice c (Å)
- 10.773
Superconducting parameters
- λ_eph (e–ph coupling)
- 0.78
- ω_log
- 255 K
Samples & pressure
- Sample form
- polycrystal