Tc max
26.0 K
Tc ambient
—
arXiv year
2001
Papers
2
Tc exp.
26.0 K
Tc theo.
24.5 K
Evidence
mixed
Tc max measured at polycrystal, susceptibility, DOI: 10.1103/PhysRevLett.86.5775
Evidence (3 records from 2 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 26.0 | — | polycrystal | susceptibility | — | 2001 | T1 | DOI: 10.1103/PhysRevLett.86.5775 |
| 24.5 | — | — | — | — | 2002 | T1 | cond-mat/0204580 |
| 0.5 | — | — | — | — | 2002 | T1 | cond-mat/0204580 |
Superconducting parameters
- λ_eph (e–ph coupling)
- —