Tc max
6.0 K
Tc ambient
6.0 K
arXiv year
2009
Papers
11
Tc exp.
6.0 K
Tc theo.
—
Evidence
experimental
Tc max measured at ambient, polycrystal, resistivity, arXiv:1003.0785, confirmed by 3 papers
Evidence (15 records from 11 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 6.0 | ambient | polycrystal | resistivity | — | 2010 | T1 | 1003.0785 |
| 6.0 | ambient | polycrystal | resistivity, susceptibility | — | 2010 | T1 | DOI: 10.1103/PhysRevB.82.014514 |
| 6.0 | 0.4 | polycrystal | resistivity, susceptibility | — | 2010 | T1 | DOI: 10.1103/PhysRevB.82.014514 |
| 6.0 | — | — | — | — | 2009 | T1 | 0908.4043 |
| 5.5 | — | polycrystal | susceptibility | — | 2010 | T1 | 1005.0494 |
| 5.0 | ambient | polycrystal | susceptibility, resistivity | — | 2014 | T1 | 1403.4458 |
| 5.0 | — | polycrystal | specific_heat | — | 2013 | T1 | DOI: 10.1103/PhysRevB.87.054504 |
| 5.0 | — | single_crystal | resistivity | — | 2011 | T1 | 1112.5597 |
| 4.9 | — | single_crystal | susceptibility | unknown | 2012 | T1 | DOI: 10.1103/PhysRevLett.108.047002 |
| 4.9 | — | single_crystal | susceptibility | — | 2011 | T1 | 1107.4375 |
| 4.9 | — | polycrystal | specific_heat | — | 2013 | T1 | DOI: 10.1103/PhysRevB.87.054504 |
| 4.7 | — | single_crystal | susceptibility | unknown | 2012 | T1 | DOI: 10.1103/PhysRevLett.108.047002 |
| 4.7 | — | single_crystal | susceptibility | — | 2011 | T1 | 1107.4375 |
| 4.5 | — | single_crystal | susceptibility | — | 2012 | T1 | DOI: 10.1103/PhysRevLett.108.047003 |
| — | — | — | — | — | 2011 | — | 1108.3956 |
Structure
- Crystal structure
- Cu2Sb structure
- Space group
- P4/nmm
- Lattice a (Å)
- 3.694
- Lattice c (Å)
- 6.045
Superconducting parameters
- Gap structure
- nodal
- λ_eph (e–ph coupling)
- —
Competing orders
- ρ(T) exponent
- 2.00
Samples & pressure
- Sample form
- polycrystal