Tc max
23.0 K
Tc ambient
23.0 K
Discovery
2004
Papers
2
Tc max measured at ambient, polycrystal, susceptibility, arXiv:cond-mat/0411149
Evidence (2 records from 2 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Paper |
|---|---|---|---|---|---|---|
| 23.0 | ambient | polycrystal | susceptibility | — | 2004 | cond-mat/0411149 |
| — | ambient | polycrystal | magnetization, resistivity | — | 2004 | cond-mat/0410722 |
Superconducting parameters
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- polycrystal
- Doping level
- 0.200