Tc max
37.0 K
Tc ambient
37.0 K
arXiv year
2001
Papers
11
Tc exp.
37.0 K
Tc theo.
—
Evidence
experimental
Tc max measured at single_crystal, resistivity, arXiv:cond-mat/0411449, confirmed by 4 papers
Evidence (23 records from 11 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 37.0 | — | single_crystal | resistivity | — | 2004 | T1 | cond-mat/0411449 |
| 35.9 | — | single_crystal | susceptibility | — | 2005 | T1 | DOI: 10.1103/PhysRevB.71.174506 |
| 35.6 | — | single_crystal | susceptibility | — | 2005 | T1 | DOI: 10.1103/PhysRevB.71.174506 |
| 35.1 | — | single_crystal | susceptibility | — | 2005 | T1 | DOI: 10.1103/PhysRevB.71.174506 |
| 35.0 | — | single_crystal | susceptibility | — | 2005 | T1 | DOI: 10.1103/PhysRevB.71.174506 |
| 34.8 | — | single_crystal | susceptibility | — | 2005 | T1 | DOI: 10.1103/PhysRevB.71.174506 |
| 34.6 | — | single_crystal | susceptibility | — | 2005 | T1 | DOI: 10.1103/PhysRevB.71.174506 |
| 34.0 | — | single_crystal | susceptibility | — | 2005 | T1 | DOI: 10.1103/PhysRevB.71.174506 |
| 33.1 | — | single_crystal | susceptibility | — | 2005 | T1 | DOI: 10.1103/PhysRevB.71.174506 |
| 32.6 | — | single_crystal | susceptibility | — | 2005 | T1 | DOI: 10.1103/PhysRevB.71.174506 |
| 31.8 | — | single_crystal | susceptibility | — | 2005 | T1 | DOI: 10.1103/PhysRevB.71.174506 |
| 29.9 | — | single_crystal | susceptibility | — | 2005 | T1 | DOI: 10.1103/PhysRevB.71.174506 |
| 20.0 | — | single_crystal | resistivity | — | 2004 | T1 | cond-mat/0411449 |
| 18.0 | — | single_crystal | — | — | 2006 | T1 | cond-mat/0604316 |
| 12.5 | — | single_crystal | — | — | 2006 | T1 | cond-mat/0604316 |
| 7.0 | — | polycrystal | susceptibility, specific_heat | — | 2005 | T1 | DOI: 10.1103/PhysRevLett.95.267002 |
| — | — | — | — | s-wave | 2010 | T1 | DOI: 10.1103/PhysRevB.82.224508 |
| — | — | single_crystal | susceptibility, STM | — | 2004 | T1 | cond-mat/0407267 |
| — | — | — | muSR | — | 2004 | T1 | cond-mat/0401454 |
| — | — | polycrystal | susceptibility | s-wave | 2002 | T1 | DOI: 10.1103/PhysRevB.66.064516 |
| — | — | polycrystal | susceptibility | — | 2002 | T1 | DOI: 10.1103/PhysRevB.65.214536 |
| — | — | polycrystal | susceptibility, resistivity | — | 2002 | T1 | cond-mat/0206409 |
| — | — | — | resistivity | — | 2001 | T1 | cond-mat/0104366 |
Superconducting parameters
- Pairing symmetry
- s-wave
- Gap structure
- multi_gap
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- single_crystal
- Pressure type
- none
- Doping type
- electron
- Doping level
- 0.035