Tc max
36.6 K
Tc ambient
36.6 K
Discovery
2002
Papers
1
Tc max measured at ambient, polycrystal, susceptibility, arXiv:cond-mat/0207093
Evidence (1 record from 1 paper)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Paper |
|---|---|---|---|---|---|---|
| 36.6 | ambient | polycrystal | susceptibility | — | 2002 | cond-mat/0207093 |
Structure
- Crystal structure
- hexagonal AlB2-type
- Space group
- P6/mmm (#191)
Superconducting parameters
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- polycrystal
- Pressure type
- none
- Doping type
- isovalent
- Doping level
- 0.800