Tc max
7.5 K
Tc ambient
7.5 K
arXiv year
2002
Papers
2
Tc exp.
7.5 K
Tc theo.
—
Evidence
experimental
Tc max measured at polycrystal, susceptibility, arXiv:cond-mat/0209077, confirmed by 2 papers
Evidence (3 records from 2 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 7.5 | — | polycrystal | susceptibility | — | 2002 | T2 | cond-mat/0209077 |
| 6.8 | — | polycrystal | susceptibility | — | 2002 | T2 | cond-mat/0209077 |
| 6.5 | — | single_crystal | susceptibility | — | 2019 | — | 1905.06909 |
Structure
- Crystal structure
- cubic antiperovskite
- Space group
- Pm-3m (#221)
- Lattice a (Å)
- 3.791
Superconducting parameters
- λ_eph (e–ph coupling)
- —