Tc max
4.7 K
Tc ambient
4.7 K
arXiv year
2004
Papers
2
Tc exp.
4.7 K
Tc theo.
—
Evidence
experimental
Tc max measured at powder, susceptibility, arXiv:cond-mat/0407192, confirmed by 2 papers
Evidence (3 records from 2 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 4.7 | — | powder | susceptibility, NQR | — | 2004 | T1 | cond-mat/0407192 |
| 3.9 | — | powder | NQR | — | 2004 | T1 | cond-mat/0407192 |
| 2.8 | — | — | — | — | 2004 | T1 | cond-mat/0410478 |