Tc max
7.4 K
Tc ambient
7.4 K
arXiv year
2010
Papers
8
Tc exp.
7.0 K
Tc theo.
—
Evidence
experimental
Tc max measured at ambient, polycrystal, susceptibility, DOI: 10.1103/PhysRevB.86.174522, confirmed by 3 papers
Evidence (11 records from 8 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 8.8 | 3.5 | polycrystal | resistivity | — | 2012 | T1 | DOI: 10.1103/PhysRevB.86.174522 |
| 8.6 | 2.0 | polycrystal | susceptibility | — | 2012 | T1 | DOI: 10.1103/PhysRevB.86.174522 |
| 7.4 | ambient | polycrystal | susceptibility | — | 2012 | T1 | DOI: 10.1103/PhysRevB.86.174522 |
| 7.3 | 0.5 | polycrystal | resistivity | — | 2012 | T1 | DOI: 10.1103/PhysRevB.86.174522 |
| 7.0 | ambient | — | muSR | s-wave | 2019 | T1 | 1909.06875 |
| 7.0 | — | — | — | — | 2010 | T1 | 1001.0665 |
| 6.8 | — | single_crystal | resistivity, susceptibility, specific_heat | — | 2021 | T1 | 2102.09782 |
| 6.8 | — | single_crystal | resistivity | — | 2021 | T1 | 2112.07866 |
| — | — | — | STM | s-wave | 2026 | T1 | 2601.13063 |
| — | — | single_crystal | STM | — | 2026 | T1 | DOI: 10.1103/qfqm-qp82 |
| — | — | — | STM | — | 2024 | T1 | 2403.01949 |
Structure
- Crystal structure
- PbFCl-type
- Space group
- P4/nmm (129)
- Lattice a (Å)
- 4.125
- Lattice c (Å)
- 7.368
Superconducting parameters
- Pairing symmetry
- s-wave
- λ_eph (e–ph coupling)
- —
Competing orders
- ρ(T) exponent
- 2.00
Samples & pressure
- Pressure type
- none