Tc max
20.2 K
Tc ambient
20.2 K
arXiv year
2012
Papers
4
Tc exp.
20.2 K
Tc theo.
—
Evidence
experimental
Tc max measured at single_crystal, resistivity, arXiv:1204.3440, confirmed by 3 papers
Evidence (5 records from 4 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 20.2 | — | single_crystal | resistivity | — | 2012 | T1 | 1204.3440 |
| 20.0 | — | single_crystal | susceptibility | — | 2012 | T1 | 1204.3440 |
| 20.0 | — | single_crystal | resistivity, susceptibility, specific_heat | s-wave | 2012 | T1 | 1204.3522 |
| 20.0 | ambient | single_crystal | resistivity, susceptibility, specific_heat | — | 2012 | T2 | 1207.5382 |
| — | — | single_crystal | susceptibility | — | 2012 | T1 | DOI: 10.1103/PhysRevB.86.020508 |
Structure
- Crystal structure
- Fe2As structure
Superconducting parameters
- Hc2
- 36.0 T (defined by ρ = 0)
- λ_eph (e–ph coupling)
- —
Competing orders
- ρ(T) exponent
- 1.00
Samples & pressure
- Sample form
- single_crystal
- Doping level
- 0.028