Tc max
6.0 K
Tc ambient
6.0 K
arXiv year
2023
Papers
2
Tc exp.
6.0 K
Tc theo.
16.3 K
Evidence
experimental
Tc max measured at polycrystal, resistivity, DOI: 10.1103/PhysRevB.108.174517
Evidence (6 records from 2 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 16.3 | — | — | — | s-wave | 2023 | T1 | DOI: 10.1103/PhysRevB.108.054519 |
| 6.0 | — | polycrystal | resistivity | s-wave | 2023 | T1 | DOI: 10.1103/PhysRevB.108.174517 |
| 5.5 | — | polycrystal | resistivity | s-wave | 2023 | T1 | DOI: 10.1103/PhysRevB.108.174517 |
| 5.2 | — | polycrystal | resistivity | s-wave | 2023 | T1 | DOI: 10.1103/PhysRevB.108.174517 |
| 5.1 | — | polycrystal | specific_heat | s-wave | 2023 | T1 | DOI: 10.1103/PhysRevB.108.174517 |
| 4.8 | — | polycrystal | susceptibility | s-wave | 2023 | T1 | DOI: 10.1103/PhysRevB.108.174517 |
Structure
- Crystal structure
- NiAs-type
- Space group
- P63/mmc (No. 194)
- Lattice a (Å)
- 3.290
- Lattice c (Å)
- 6.670
Superconducting parameters
- Pairing symmetry
- s-wave
- Gap structure
- full_gap
- Hc2
- 7.4 T (0 K, from Tconset)
- λ_eph (e–ph coupling)
- 1.31
- ω_log
- 184 K