← Materials
Nd0.825Sr0.175NiO2
nickelate · infinite-layer · infinite_layer
ambient SCunconventionaldisputed
Tc max
16.5 K
Tc ambient
15.0 K
arXiv year
2021
Papers
4
Tc exp.
16.5 K
Tc theo.
—
Evidence
experimental
Tc max measured at thin_film, resistivity, DOI: 10.1103/7lqb-pjkm, confirmed by 2 papers
Evidence (6 records from 4 papers)
the flat columns above are aggregates — each line here is one paper's claim| Tc (K) | P (GPa) | Sample | Method | Pairing | Year | Tier | Paper |
|---|---|---|---|---|---|---|---|
| 16.5 | — | thin_film | resistivity | — | 2025 | T1 | DOI: 10.1103/7lqb-pjkm |
| 15.0 | — | thin_film | resistivity | — | 2023 | T1 | 2309.03170 |
| 13.6 | — | thin_film | resistivity | — | 2025 | T1 | DOI: 10.1103/7lqb-pjkm |
| 6.1 | — | thin_film | resistivity | — | 2023 | T1 | 2309.03170 |
| — | — | thin_film | — | unknown | 2025 | T1 | 2506.09543 |
| — | — | thin_film | resistivity | — | 2021 | T1 | 2105.07783 |
Structure
- Crystal structure
- infinite-layer
- Phase
- infinite_layer
Superconducting parameters
- λ_eph (e–ph coupling)
- —
Samples & pressure
- Sample form
- thin_film
- Substrate
- LSAT
- Doping type
- hole
- Doping level
- 0.175